Conductivity and dielectric properties of SrLaxBixYxFe12-O-3x(19) (0.0 <= x <= 0.33) hexaferrites

dc.contributor.authorBakis, Y.
dc.contributor.authorAuwal, I. A.
dc.contributor.authorÜnal, Bayram
dc.contributor.authorBaykal, A.
dc.date.accessioned2019-08-31T12:10:23Z
dc.date.accessioned2019-08-13T09:37:48Z
dc.date.available2019-08-31T12:10:23Z
dc.date.available2019-08-13T09:37:48Z
dc.date.issued2016en_US
dc.departmentMühendislik ve Doğa Bilimleri Fakültesien_US
dc.descriptionWOS: 000377733500036en_US
dc.description.abstractBoth Y-La-Bi substituted and non-substituted Sr-hexaferrites (SrM) were synthesized by sol-gel auto combustion technique and the influences of Y, La and Bi ions on ac/dc conductivities, dielectric constant/loss properties as well as complex dielectric modulus were investigated extensively for a variety of substitutions. It was observed that ac conductivity of SrM increases slightly with increasing Y3+ La-3, and Bi3+ substitutions at first, and then decreases with its further increments. Furthermore, ac conductivity increased with increasing frequency which could be regarded as an origin indication of both electronic and polaron hopping mechanism. It is also worthy to note that the activation energy, which is an indication of both mechanisms depicted in the Arrhenius plot, is increased as the enhanced contributions of substitutions in SrM with the illustration of a better stability and tunability of electrical bonds among substituted ions and ferrous and ferric ions. The dielectric constant, dielectric loss and dielectric modulus represent a very interesting tunability and optimised consequences regarding to the variation of frequencies, temperatures and substitutions of SrM. (C) 2016 Elsevier Ltd and Techna Group S.r.l. All rights reserved.en_US
dc.description.sponsorshipFatih University [P50031504_B (10790)]; Namik Kemal University [NKUBAP.06. GA.16.047]en_US
dc.description.sponsorshipThe authors would like to thank Fatih University (P50031504_B (10790)) and Namik Kemal University (NKUBAP.06. GA.16.047).en_US
dc.identifier.doi10.1016/j.ceramint.2016.04.099
dc.identifier.endpage11795en_US
dc.identifier.issn0272-8842
dc.identifier.issn1873-3956
dc.identifier.issue10en_US
dc.identifier.orcidBayram Ünal |0000-0003-2025-9848en_US
dc.identifier.scopusqualityQ1
dc.identifier.startpage11780en_US
dc.identifier.urihttp://dx.doi.org/10.1016/j.ceramint.2016.04.099
dc.identifier.urihttps://hdl.handle.net/20.500.12436/1043
dc.identifier.volume42en_US
dc.identifier.wosqualityN/Aen_US
dc.indekslendigikaynakWeb of Science
dc.indekslendigikaynakScopus
dc.institutionauthorÜnal, Bayram
dc.language.isoen
dc.publisherELSEVIER SCI LTDen_US
dc.relation.ispartofCERAMICS INTERNATIONALen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/openAccessen_US
dc.subjectHexaferritesen_US
dc.subjectElectrical conductivityen_US
dc.subjectDielectric constanten_US
dc.subjectDielectric lossen_US
dc.subjectResistivityen_US
dc.titleConductivity and dielectric properties of SrLaxBixYxFe12-O-3x(19) (0.0 <= x <= 0.33) hexaferritesen_US
dc.typeArticle
dspace.entity.typePublication

Dosyalar

Orijinal paket

Listeleniyor 1 - 1 / 1
Yükleniyor...
Küçük Resim
İsim:
Conductivity_and_dielectric_properties_of_SrLaxBix.pdf
Boyut:
11.9 MB
Biçim:
Adobe Portable Document Format
Açıklama:
Tam Metin / Full Text